Film Thickness

Film thickness is the measured depth of an anodic or organic coating, specified as a minimum class and checked on significant surfaces.

Every Film Thickness article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Film thickness is the measured depth of an anodic or organic coating, specified as a minimum class and checked on significant surfaces.

Anodic Film

Hydro anodizes extruded profiles until the desired film thickness is reached, generally up to 25 µm (0.98 mil), and recommends 10 to 25 µm by exposure, with at least 20 µm (0.79 mil) for color anodizing. The Aluminum Association system, as the Aluminum Anodizers Council reproduces it, sets Architectural Class II at 0.4 to 0.7 mil (10.2 to 17.8 µm) and Class I at 0.7 mil (17.8 µm) and thicker.
Read More

Acceptance Rules

ISO 7599:2018 grades anodic coatings by minimum average thickness, from AA 5 to AA 25 in its typical classes, and never lets the minimum local thickness fall below 80 % of that average, so AA 20 carries a local floor of 16 µm (0.63 mil). Readings are taken on significant surfaces, never within 5 mm (0.2 in) of the areas of anodic contact or near a sharp edge.

Organic Coatings

The PCI comparison lists Qualicoat powder minimums of 60 µm (2.4 mil) for Classes 1 and 2 and 50 µm (2.0 mil) for Class 3, and AAMA minimums of 20 µm (0.8 mil) for 2603 and 30 µm (1.2 mil) for 2604 and 2605. AAMA 605-98 noted that inside corners and channels of an extrusion may not reach the minimum.

Dimensional Effect

Film adds to the extruded size. EN 12020-2 applies to profiles without further surface treatment, so a slot or snap fit carries its film on top of the extrusion tolerance.

Anodizing Extruded Aluminum Profiles Step by Step

Anodizing an extrusion is a line of tanks, and the rack, etch, bath, color and seal each leave their own mark on the profile.

The Anodizing Line From Rack to SealHydro's anodizing brochure for extruded profiles lays out the line in the order the profiles travel. The Aluminum Anodizers Council groups the same work into five stages: cleaning, pretreatment, anodizing, coloring and sealing.

Anodized Film Thickness and Color Tolerance on Extruded Profiles

Specify anodic film as an ISO 7599 class on marked faces, and agree color against limit samples before the first lot is anodized.

How Anodized Film Thickness Is Specified and AcceptedISO 7599:2018, published in Europe as EN ISO 7599:2018 and in Britain as BS EN ISO 7599:2018, lays down the method. Its contents run from the information the customer supplies to the anodizer, through coating thickness, sealing, appearance and color, to a normative annex on interpreting average and local thickness.

Qualicoat and AAMA 2603 to 2605 Coating Specifications for Aluminum Extrusions

Name the Qualicoat class or AAMA tier on the drawing, then fix the approved sample, channel thickness and machining rules that neither standard settles.

What Qualicoat and AAMA 2603, 2604 and 2605 CoverQualicoat is a quality label for coatings on aluminum for architectural use. Its 26th edition, introduced in the document QCT-INTRO-26 valid from 1 January 2026, splits the specifications into three volumes: one for coaters, one for makers of chemical pretreatments and one for powder makers.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote