Aluminum Association

The Aluminum Association is the North American industry body that writes and publishes the aluminum standards most extrusion drawings in inches cite.

Every Aluminum Association article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The Aluminum Association is the North American industry body that writes and publishes the aluminum standards most extrusion drawings in inches cite. ANSI H35.2, the dimensional tolerance standard for aluminum mill products, is administered by the Association. It also publishes Aluminum Standards and Data, with the property limits and tolerance tables extruders quote. Its letters and guides explain how those tables are read.

Standards Work

The foreword to ANSI H35.2 traces its extrusion tolerances to 1949. In that year its Extruded Products Division started work on common tolerances for extruded shapes. The foreword calls them broadly accepted across the industry and by users of the metal. It also names them the basis of tolerances in United States government and technical society specifications. The 2017 edition was approved on May 12, 2017, revising the 2013 edition.
Read More

Published Tables

Selected 2009 tables of Aluminum Standards and Data are posted by the Association at no charge. They are offered as a courtesy to users of the AEC’s Aluminum Extrusion Manual. The set covers Tables 11.5 to 11.14 for profiles and 12.2 to 12.5 and 12.10 to 12.14 for tube. Table 11.1, the property limits for extruded profiles, is printed in ksi. The cross-section limits of Table 11.2 sit in the 2017 standard itself.

Interpretation Letters

The Association answers questions on its standards in dated letters. A letter of June 6, 2025 dealt with straightness of a 0.91 m (3 ft) tube under Tables 12.8 and 12.25. Every condition applies together, it said. Any 0.30 m (1 ft) section may deviate by 0.25 mm (0.010 in), and any 0.61 m (2 ft) section by 0.51 mm (0.020 in). The whole length may deviate by 0.76 mm (0.030 in). The same letter declined to compare the ANSI H35.2 method with straightness per unit length under ASME Y14.5.

Video Guide

A video series, Understanding Aluminum Extrusion Tolerances, walks through the tables feature by feature. It explains metal and space dimensions and sends solid profiles to Table 11.2. For tube and hollow profiles it adds Tables 12.2, 12.3 and 12.4. Twist is described as rotation about the long axis, with Tables 10.14, 11.7, 12.7, 12.26 and 12.46. Flatness applies across the width only, with separate limits for solid and hollow sections.

Average Profile Clause

The Association’s tolerances carry a footnote that shapes every reading. The printed limits are those of an average profile. A demanding section may need more room, and a simple one may hold less. The footnote expects the buyer and the extruder to go through each section’s critical features jointly. The AEC adds that many extruders can work closer than the tables. The tables open the conversation, and the drawing records where it ended. A closer limit agreed with one extruder becomes a line on the drawing and leaves the standard as it is.

Footnote Rules

The footnotes to the Association’s tolerance tables carry rules a buyer meets on every drawing. TX510 and TX511 are named there as the two umbrella codes for stress-relieved tempers, such as T6510 and T6511. For the TX510 group, form values are left to agreement between purchaser and vendor. The O temper is allowed four times the standard flatness. Straightness is measured with the piece on a flat surface, in the position where its weight gives the least deviation. The limit then has to hold in every orientation, including those where the piece cannot carry its own weight.

Two Systems

The Association’s limits are not interchangeable with the European ones. Its 6063-T5 band ends at 12.7 mm (0.500 in), where Hydro’s EN 755-2 band ends at 10 mm (0.39 in). A 14 mm (0.55 in) 6063-T5 wall reads 103 MPa (15.0 ksi) yield in the Association’s table. Hydro’s EN 755-2 table gives the same wall 110 MPa (16.0 ksi). A lot can meet one table and miss the other, so the order names one. The AEC die life table also assumes the Association’s standard dimensional tolerances.

Anodizing Extruded Aluminum Profiles Step by Step

Anodizing an extrusion is a line of tanks, and the rack, etch, bath, color and seal each leave their own mark on the profile.

The Anodizing Line From Rack to SealHydro's anodizing brochure for extruded profiles lays out the line in the order the profiles travel. The Aluminum Anodizers Council groups the same work into five stages: cleaning, pretreatment, anodizing, coloring and sealing.

Anodized Film Thickness and Color Tolerance on Extruded Profiles

Specify anodic film as an ISO 7599 class on marked faces, and agree color against limit samples before the first lot is anodized.

How Anodized Film Thickness Is Specified and AcceptedISO 7599:2018, published in Europe as EN ISO 7599:2018 and in Britain as BS EN ISO 7599:2018, lays down the method. Its contents run from the information the customer supplies to the anodizer, through coating thickness, sealing, appearance and color, to a normative annex on interpreting average and local thickness.

EN 755-9 and EN 12020-2 Scope and Editions for Aluminum Extruded Profiles

Name EN 755-9 or EN 12020-2 with its year, because scope, alloys and limits differ by standard and edition.

What EN 755-9 and EN 12020-2 Each CoverEN 755-9 is part 9 of the EN 755 series for extruded rod and bar, tube and profiles. BSI describes BS EN 755-9:2016 as specifying the tolerances on dimensions and form for aluminum and aluminum alloy profiles with a cross-section contained within a circumscribing circle not greater than 800 mm.

Cut Length and Saw Cut Tolerance of Extruded Profiles

A length tolerance belongs to a cutting step and a measuring method, so name both with the number.

Saw Tolerances for Plastic Profile LengthsBWF's guidelines of 20 November 2024 give saw tolerances for polycarbonate and PMMA profiles in two cases, offline cut and inline cut. Each is tabulated against the length, in millimeters, and each is tied to a method: lengths up to 4,500 mm are measured on a measuring table that checks length and angle, and longer ones with a measuring tape.

Straightness, Twist and Flatness Tolerance of Aluminum Extrusions

Form limits scale with length and width, so work them out for the real length before accepting a drawing.

The Straightness Limit and Its FormulaTable 11.6 of Aluminum Standards and Data, in the May 2009 reprint, gives the allowable deviation D from straight in inches. For profiles the limit is a factor multiplied by the measured length in feet, and it applies in total length or in any measured segment of one foot or more of the total length.

ASTM B221 for Extruded Aluminum Profiles Read for the Buyer

The specification certifies alloy, temper and tensile behavior, so the drawing still has to carry geometry, units and thickness.

What ASTM B221 CoversASTM's catalog page for B221-21, last updated October 29, 2021, describes the standard as a specification for aluminum and aluminum-alloy extruded bars, rods, wire, profiles and tubes. It covers the alloys and tempers listed in its Table 2 and requires the products to be made by hot extrusion or a similar process.

ANSI H35.2 Standard Tolerances for Aluminum Extrusions

Name the edition and the class on the drawing, because the standard column governs when nothing is written.

What ANSI H35.2 Covers and How to Cite ItThe title is American National Standard Dimensional Tolerances for Aluminum Mill Products, and the Aluminum Association is its secretariat. Opened for this piece was ANSI H35.2-2017, approved May 12, 2017 as a revision of the 2013 edition, in the December 2017 errata issue.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.