Exposure is the environment a profile meets in service or in a test, such as sun, weather, chemicals or a corrosive atmosphere, stated with its duration. For extruded profiles it sets the class of a finish and the family of a seal compound.Florida Exposure
Coating classes are proven on outdoor fences in South Florida. The PCI comparison lists one year for Qualicoat Class 1, three years for Class 2 and ten years for Class 3, and one, five and ten years for AAMA 2603, 2604 and 2605. The BNP Media course places the AAMA 2605 fence south of latitude 27° N, tilted 45° facing south. PPG cites, for 2605 after ten years, fade within 5 ΔE, chalk of 8 or better and 50 % gloss retention.Read More
Anodizing
Hydro recommends anodic film thickness by exposure: 10 µm (0.39 mil) for normal indoor use, 20 µm (0.79 mil) for normal to high stress outdoors and 25 µm (0.98 mil) for corrosive or abrasive exposure. Some inorganic dyes have limited fastness and do not suit high temperature or strong UV exposure.Seal Compounds
Trelleborg lists UV and weather exposure beside temperature range, chemical compatibility and compression among the bases of seal material selection. Teknor Apex’s worksheet asks whether a chemical only splashes the part or submerges it, and at what temperature. Elastron rates its SBS-based TPE line poor for UV, against good for its SEBS and TPV lines.Order Wording
Exposure is written as a condition with a time: the site or cabinet, the duration and the property checked afterward.