Minimum Exit Weight

The minimum exit weight is the lowest weight per meter an aluminum press line can handle on its puller and run-out table.

Every Minimum Exit Weight article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The minimum exit weight is the lowest weight per meter an aluminum press line can handle on its puller and run-out table. A single profile lighter than that cannot be run alone. It is one reason small profiles share a die.

Why It Exists

Hydro states the limit in terms of the downstream equipment. Below a certain weight per meter, the strand is too light for the puller to draw and the table to carry. The constraint therefore comes from handling the strand, not from forming it at the die.
Read More

Multi-Cavity Answer

The usual answer is a die with several openings. Hydro names up to 16 openings for small, light profiles. The strands leave together and pass the limit as a group. Large and medium profiles keep a single opening, where flow and tolerance are easier to control.

Choosing the Cavity Count

Hydro’s engineers set the number of openings from several factors. Press tonnage, alloy, geometry and downstream handling all enter the choice. How die life scales with more openings is not given in the AEC table. That question goes to the extruder for each multi-cavity tool.

What It Does Not Change

More openings give more length per stroke, so press time for a given weight falls. The weight an order carries against the extruder’s minimum stays the same. A smaller press with smaller billets is the other lever for a small quantity. For a light profile of about 1 kg per meter, the smallest published batch already exceeds 200 m.

Aluminum Extrusion Die Life in Kilograms Before the Bearing Wears

Die life is counted in tonnes of aluminum before the bearing wears, so a bridge run usually needs one die and a plan for its trial and correction.

What Wears an Extrusion Die and How FastThe AEC manual explains that the life of an extrusion die is generally set by wear of the bearing, the surface of the die opening at right angles to the die face that controls metal flow and velocity by friction. Because the bearing determines the control and finish of the profile, any deterioration, given the finish required, leads to premature failure of the die.

How Much of an Aluminum Billet Becomes Shipped Profile

Order weight, butt, stretcher ends and rejects decide how many billets a small aluminum extrusion run takes and what the buyer receives.

The Yield Stack From Billet to Shipped LengthA billet is heated, pushed through a die, quenched, stretched, sawn and aged. Metal leaves the stream at three points, and each has a figure in the published sources.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.