One saw maker reports that changing the kerf of a carbide blade from 4.6 mm to 2.5 mm raised the yield of a six-meter aluminum bar from 410 pieces to 480, with the same cut quality and blade life. Working backward, those figures fit pieces about 10 mm long, so the saw’s cut width is a measurable share of what the bar delivers. The article does not print the piece length; the 10 mm is arithmetic on its two counts, and it shows why a kerf is not an afterthought on short parts.
An extruded bar is rarely the part. It is a long, straight, near-net shape that leaves the press at around 5.5 m (18 ft) in one extruder’s practice, and it becomes a part when it is cut to length, deburred and given holes, slots or threads. Each of those steps has a published habit that keeps a thin wall flat and a hole round, and each has a symptom when the habit slips. The sections below follow the order in which a length is made.
The Order of Operations From Bar to Cut Length
Cutting comes first in almost any fabrication plan, with deburring and then drilling, punching or machining after it. A burr left from the cut sits where the clamp has to hold the piece for the next step, so the order carries weight.
| Step | Operation | What it controls | Source |
|---|---|---|---|
| 1 | Saw the bar to rough length at the press | trims stretcher grip marks and the front and back ends | University of Illinois thesis |
| 2 | Gauge the first pieces | inner and outer diameter, length, flatness | Alliance process sheet |
| 3 | Cut again to the ordered length on a precision saw | cut length and squareness | alcircle guide to fabrication |
| 4 | Deburr | edges at cut ends, holes and slots | alcircle guide to fabrication |
| 5 | Drill, punch, mill or tap | features on one or several faces | AEC Aluminum Extrusion Manual |
| 6 | Finish | anodize, coat or leave mill finish | AEC process page |
Different jobs fall to the press saw and the precision saw. Standard lengths, and the removal of unusable ends, belong to the first. The lengths a drawing asks for belong to the second.
The press saw cuts the bar to a length the extruder can ship. The precision saw cuts the length the drawing asks for, and it is the one that decides how much burr work follows.
What the Press Saw Does
An Alliance process sheet describes bars of about 18 ft (5.5 m) cut to specific lengths on a saw table after stretching. It gives a standard cutting tolerance on those saws of 0.125 in. (3.2 mm) or greater, depending on saw length, and adds that the ends of the bar are usually not to tolerance and are removed as scrap. In a University of Illinois thesis on extrusion modeling, the saw is a high-speed circular saw, with the sections moved against a gauge stop set to the required length, chips collected by a high-pressure vacuum and several extrusions cut at once where the section, the alloy and the saw allow. Any drawing that asks for a tighter cut length than 3.2 mm calls for a second cut on a precision saw, or for a machined end.
How a Saw Cuts Aluminum and Where the Burrs Come From
Aluminum is soft and ductile, so a tooth does not slice it like scissors. According to a German saw maker’s guide on low-burr cutting, the wedge-shaped tooth makes the metal deform plastically and compress ahead of the edge before it shears off as a chip. Three burrs follow from that: a small entry burr where the tooth enters, a side burr from metal displaced into the sides of the kerf, and an exit burr on the underside where the tooth leaves and the unsupported metal bends downward instead of shearing. The same guide names the exit burr as the largest and the most troublesome.
Blade Geometry
Vendor documents agree on a short list of blade features for extrusions. A triple-chip grind splits the work between a roughing tooth and a finishing tooth. Negative hook angle, typically minus 5 to minus 6 degrees in the German guide, makes the tooth scrape under control. And a high tooth count keeps several teeth in contact so that a thin wall is not bent between two far-spaced teeth. Amana lists a 7 in. (178 mm) carbide-tipped blade with 58 teeth, a triple-chip grind and a minus 6 degree hook as suited to thin-walled extrusions and frames.
| Feature | What it does | Source |
|---|---|---|
| Triple-chip grind | divides cutting between a roughing and a finishing tooth | Evomatec low-burr cutting guide |
| Negative hook angle (minus 5 to minus 6 degrees) | tooth scrapes instead of digging in | Evomatec; Amana |
| High tooth count | keeps a thin wall supported by several teeth at once | Evomatec |
| Sharp edge | a dull edge squeezes metal and raises burr formation | Evomatec |
| Reduced kerf (4.6 mm to 2.5 mm) | more pieces per bar at the same cut quality | Moreschi |
| Thin-wall support with adjustable pressure | holds the profile without crushing hollows | Evomatec; alcircle |
Every figure in the table is a maker’s statement about its own blade or machine. None of them is a measured comparison across suppliers, and the sources do not give a cutting speed or a feed rate in a unit a buyer could check. For that reason, a drawing never specifies a blade, and a buyer reads a cut by what it looks like.
Where a Saw Maker Can Move the Yield
The kerf example at the head of this piece comes from Moreschi’s report on photovoltaic profiles. Moreschi’s report also describes work on painted window and door profiles where changing tooth geometry and cutting parameters cleaned up cuts that had been damaging the coating and creating burrs, and a third case where the blade delivered a surface that removed grinding and deburring downstream. As a supplier’s account of its own projects, it carries a bias. It is still a useful reminder that a cut face is a product of tool and parameters, and that the answer to a rough cut is often found at the saw.
Holding the Profile While It Is Cut
Extrusions are long, thin-walled and sometimes asymmetrical. Alcircle’s guide to post-extrusion fabrication warns that excessive clamping pressure can deform the profile, while too little support lets it vibrate and cut inaccurately, and it recommends fixtures that support the piece close to the cut without damaging visible surfaces.
Details come from the saw guide. The profile is clamped as close as possible to the cut and on both sides of the blade, so the piece that falls away does not tilt at the last moment and tear an exit burr. Vertical and horizontal clamps together stop movement in every direction, and thin or hollow profiles need adjustable clamp pressure. A minimum quantity lubrication system forms a thin film that prevents built-up edge, which is aluminum welding itself to the carbide.
- Clamps on both sides of the blade, close to the cut line.
- Pressure set low enough for a hollow chamber, high enough to stop movement.
- A sharp blade and a lubricant film against built-up edge.
- Support under the exit side so the last of the wall is not left to bend.
The same guide says a manual chop saw cannot deliver a consistently burr-free cut with process reliability, because the feed is uncontrolled and the clamping simple. It places semi-automatic up-cut saws as the base for professional low-burr cutting, with CNC saws and double miter saws adding controlled stops on top. This is a vendor’s ranking of its own machine class, but it points to the right question to ask a supplier: how is the profile fed and held, not only what blade is used.
Drilling, Tapping and Milling Features
Once the length is cut, features go in. The AEC manual’s machining guidance says that aluminum extrusions may be machined quickly with some modification of conventional practice. Smooth surfaces come from finishing the cutting tools with considerably more side and top rake than is used on most metals, and softer alloys such as 3003 and 6063 call for large rake angles and light cuts. Water-soluble and oil-based cutting lubricants are both listed as usable.
Workholding and Datums
Alcircle’s guide separates the natural tolerance of the extruded shape from the tolerance of a machined feature. It recommends that machined features be referenced from clearly defined datums and not from an uncontrolled or cosmetic surface, and that the drawing says which dimensions come from machining and which stay inside normal extrusion tolerance. A multi-face machining center can work on several faces in one setup, which keeps those features related to each other.
Tapping and Self-Tapping Screws
For threads the choices split. Cut tapping removes material and makes chips that have to be cleared, and blind holes need depth below the usable thread to hold the lead of the tap and the chips. Form tapping displaces the metal and makes no chips, needs a different pilot hole diameter, and generally produces higher torque than cut tapping. The AEC manual also shows an alternative that skips tapping: extruding screw slots into the profile for Type F self-tapping screws, with a table pairing screw sizes with slot widths, for example a 0.164 in. (4.2 mm) outside diameter screw with a slot of 0.147 in. (3.7 mm) plus 0.007 in. (0.18 mm).
| Step | What the drawing has to say | What shows when it is missing |
|---|---|---|
| Cut length | length, squareness, and whether burrs are allowed | burr under a clamp; a gap at an assembly joint |
| Drilled hole | datum and tolerance, and which face | holes that wander from a cosmetic edge |
| Tapped hole | cut or formed thread, blind or through, depth | a bottomed tap or chips left in a blind hole |
| Slot or pocket | datum, depth and corner radius | chatter and a rough wall in thin sections |
| Deburr | which edges, how far | sharp edges on handled or anodized parts |
The entries in the third column are what the sources describe in general terms. None of them is a measured rate. At this step the profile has become a machined part, and a length with many pockets, bores and tapped holes is quoted much like machined aluminum cut from bar, only with most of the section already in place.
Stress Relief and Parts That Move
An extrusion carries residual stress from the quench and the stretch. Remove metal and the stress redistributes, and an asymmetrical part can bend as it is machined. According to the AEC manual, parts to be machined, and asymmetrical shapes that will be cut to size, should be ordered in a stress-relieved temper such as TX511 if the final parts have to hold close tolerances. TX511 appears in the manual only as an example, so a buyer asks which stress-relieved temper the supplier holds for the alloy in use and writes that temper in full on the drawing.
Why Short Pieces Make Kerf and Burr Matter More
Arithmetic shows why the Moreschi example is sensitive. A bar of length B cut into pieces of length L with a kerf K gives about B divided by L plus K pieces. For a 6,000 mm bar and a 10 mm piece, a 4.6 mm kerf gives 410 pieces and a 2.5 mm kerf gives 480, which matches the report. Pieces of 500 mm see the same change leave the count at 11, and nothing is gained.
That is a calculation on assumed lengths, not a published result, but it carries a rule a buyer can use. Kerf and burr control are a yield question on short pieces and a quality question on long ones. A program that cuts many short blanks from each bar, such as spacers or brackets, will see the saw’s kerf in its material usage, and one that cuts a few long lengths will see the burr in its assembly.
On a 10 mm piece the saw takes nearly a third of the bar. On a 500 mm piece it takes about one percent.
Gauging the Cut Lengths
An Alliance process sheet lists the final checks on extruded parts as gauging of inner diameter, outer diameter, length and flatness before packaging. The Illinois thesis assumes that quality scrap in an extrusion plant is on the order of 6 percent of the parts, and it keeps that as a planning allowance for non-conforming pieces. Those figures describe a planning model and not a guarantee, but a buyer ordering a few hundred pieces can read them as a reason to ask for a few extra.
Cutting Plastic Profile Lengths
The same questions come up on plastic lengths, but with different tools. A rigid PVC processing guide lists sharp saws, fly knives and guillotines for cutting profiles, and a process control paper adds that a circular saw on a carriage that moves with the haul-off is the usual answer for straight lengths. Where the line is too fast for a moving carriage, a guillotine can be used. Plastic lengths are cut on the line while moving, so length is set by the saw’s synchronization and not by a gauge stop.
What the Drawing Should Say About a Cut Length
A buyer who wants a length that goes straight into an assembly can head off most rework by writing a short list on the drawing.
- The length, with the tolerance, and whether it is cut at the press or on a precision saw.
- Burr limits on the cut ends and on the edges of holes and slots.
- Datums for every machined feature, kept off visible faces.
- The temper, written in full, with a stress-relieved temper where parts are asymmetrical or machined heavily.
- Thread type, cut or formed, for each tapped hole.
When those are written down, the cut length and its features are a repeatable step in a run. Where they are left to the supplier, each lot is a small experiment. A program that needs a few hundred cut and drilled lengths before a production tool or a dedicated machining cell is justified can bring them through low-volume profile extrusion as bridge production.
Sources and Further Reading
- Alliance LLC, Aluminum Extrusion Process (process sheet)
- Aluminum Extruders Council, Aluminum Extrusion Manual, 4th Edition (2013), Section 6, now issued by the Council as edition 4.2
- Jose Torre Nieto, Feature Based Costing of Extruded Parts, MS thesis, University of Illinois at Urbana-Champaign, 2010
- Moreschi, Reducing scrap and rework in aluminum profile cutting, expometals news, 15 July 2026
- Evomatec, Low burr cutting of aluminum
- Amana Tool, 575601 carbide tipped aluminum and non-ferrous blade, 7 in. x 58T TCG, minus 6 degree
- alcircle, Guide to post-extrusion fabrication: bending, CNC machining and tapping
- GEON Performance Materials, Rigid Vinyl Profiles Extrusion Guide
- Mike Newey, Getting critical on extrusion