Cross-Section

A cross-section is the shape an extruded profile shows when cut at right angles to its length, repeated along every meter of the run.

Every Cross-Section article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A cross-section is the shape an extruded profile shows when cut at right angles to its length, repeated along every meter of the run. On the drawing it carries the walls, widths, gaps and radii. In aluminum, it decides the die type, the press that can run it and the strength row on the certificate. In plastic, the general tolerances that one profile maker applies hold anywhere on the section, viewed across the extrusion direction.

Mixed Walls

A cross-section with walls of different thickness is graded by its weakest band. Hydro’s EN AW-6063 and EN AW-6082 datasheets both carry this footnote. When walls fall in more than one band, the whole profile takes the lowest value specified for any of them. Take a 6063 heat-sink with 3 mm (0.12 in) fins on a 12 mm (0.47 in) base. In T6 it is graded on the base, at 160 MPa (23.2 ksi) yield. Its fins alone would earn 170 MPa (24.7 ksi). A 6082-T6 hollow tube with 4 mm (0.16 in) walls and a 6 mm (0.24 in) web stays at 250 MPa (36.3 ksi). On 6005A a thicker rib lowers the guarantee, and on 6082 it leaves the thin-wall line in place.
Read More

Dimension Tolerance

ANSI H35.2-2017 Table 11.2 tolerates an aluminum section by the size of each dimension and by what it spans. A metal dimension is at least 75 % metal. A space dimension is more than 25 % open, as in the gap of a channel. Take a circumscribing circle smaller than 254 mm (10 in). There, a metal dimension of 25.4 to 38.1 mm (1.000 to 1.499 in) carries ±0.30 mm (0.012 in) at standard tolerance. The precision column gives ±0.20 mm (0.008 in). Space dimensions carry more, and they widen as the measuring point moves out from the base of the leg. On the plastic side, BWF gives a 40 mm (1.57 in) width ±0.8 mm (0.031 in). That is roughly twice the aluminum figure at the same size.

Die and Press

The cross-section sets the die before any metal moves. A shape with no void runs on a solid die. A partly enclosed void is judged by its tongue ratio. A closed void needs a hollow die, with a mandrel held on a bridge. The Aluminum Extruders Council (AEC) manual calls for a feeder plate when the section’s circle passes about 90 % of the billet diameter. A wide shape can therefore force a larger press. The extrusion ratio is billet area divided by profile area. One University of Illinois thesis puts its usual range at 10 to 100 in soft alloys and 10 to 35 in hard ones. Hydro adds that close tolerances, deep channels, varying walls and a high surface finish all lengthen die design.

Measurement

A cross-section is measured on a short piece and proved on a long one. BWF checks nominal drawing dimensions on a 50 or 100 mm (1.97 or 3.94 in) sample. It also archives a 1,000 mm (39.4 in) test piece from the start and the end of each run. A new tool is reworked in stages until the section is dimensionally and functionally accurate. The approved samples can then revise the drawing. Temperature barely moves a section of this size. A 40 mm polycarbonate width grows about 0.028 mm (0.0011 in) over a 10 °C (18 °F) rise.

Datasheet Limits

Neither a resin sheet nor an alloy sheet describes one particular cross-section. Polycarbonate values come from test specimens, so ribs, wall thickness and cooling are not in them. For aluminum, the footnotes to the Aluminum Association’s property table name the governing thickness. It is the thickness at the place the tension specimen is cut from. A property that matters at one wall is asked for as a test on the profile itself.

Drawing Callout

A dimension left without a tolerance falls to the general table of the governing standard. On aluminum, an untoleranced 100 mm (3.94 in) width reads against the 50.8 to 101.6 mm row. That row gives ±0.61 mm (0.024 in) at standard, and the drawing has to name precision to get ±0.41 mm (0.016 in). On plastic, BWF applies DIN 16941 series 2A and 2B wherever the drawing is silent. A fit between two profiles depends on several dimensions at once. The dimension that does the work is therefore toleranced directly, and the rest stay at the general limit.

EN 755-9 and EN 12020-2 Scope and Editions for Aluminum Extruded Profiles

Name EN 755-9 or EN 12020-2 with its year, because scope, alloys and limits differ by standard and edition.

What EN 755-9 and EN 12020-2 Each CoverEN 755-9 is part 9 of the EN 755 series for extruded rod and bar, tube and profiles. BSI describes BS EN 755-9:2016 as specifying the tolerances on dimensions and form for aluminum and aluminum alloy profiles with a cross-section contained within a circumscribing circle not greater than 800 mm.

Aluminum Extrusion Die Life in Kilograms Before the Bearing Wears

Die life is counted in tonnes of aluminum before the bearing wears, so a bridge run usually needs one die and a plan for its trial and correction.

What Wears an Extrusion Die and How FastThe AEC manual explains that the life of an extrusion die is generally set by wear of the bearing, the surface of the die opening at right angles to the die face that controls metal flow and velocity by friction. Because the bearing determines the control and finish of the profile, any deterioration, given the finish required, leads to premature failure of the die.

How Much of an Aluminum Billet Becomes Shipped Profile

Order weight, butt, stretcher ends and rejects decide how many billets a small aluminum extrusion run takes and what the buyer receives.

The Yield Stack From Billet to Shipped LengthA billet is heated, pushed through a die, quenched, stretched, sawn and aged. Metal leaves the stream at three points, and each has a figure in the published sources.

Wall Thickness and Cross-Section Tolerance of Extruded Plastic Profiles

Read the nominal size row for each dimension, then check the fit as a sum of limits, not a single one.

Cross-Section Dimension Limits by Nominal SizeBWF's quality, tolerance and processing guidelines of 20 November 2024 apply limit values according to DIN 16941, series 2A and 2B, unless the drawing says otherwise. The general tolerances apply at any point of the profile cross-section, seen at right angles to the extrusion direction.

Cut Length and Saw Cut Tolerance of Extruded Profiles

A length tolerance belongs to a cutting step and a measuring method, so name both with the number.

Saw Tolerances for Plastic Profile LengthsBWF's guidelines of 20 November 2024 give saw tolerances for polycarbonate and PMMA profiles in two cases, offline cut and inline cut. Each is tabulated against the length, in millimeters, and each is tied to a method: lengths up to 4,500 mm are measured on a measuring table that checks length and angle, and longer ones with a measuring tape.

DIN 16941 General Tolerances for Extruded Plastic Profiles

Cite the edition and the series on the drawing, then add what the general tolerances leave open.

What DIN 16941 CoversThe current edition is DIN 16941:2012-11, titled Thermoplastics extruded profiles, General tolerances of size, form and orientation, with the German title Extrudierte Profile aus thermoplastischen Kunststoffen, Allgemeintoleranzen für Maße, Form und Lage. It is published in German, with an English translation sold separately, and it replaces DIN 16941:1986-05.

ANSI H35.2 Standard Tolerances for Aluminum Extrusions

Name the edition and the class on the drawing, because the standard column governs when nothing is written.

What ANSI H35.2 Covers and How to Cite ItThe title is American National Standard Dimensional Tolerances for Aluminum Mill Products, and the Aluminum Association is its secretariat. Opened for this piece was ANSI H35.2-2017, approved May 12, 2017 as a revision of the 2013 edition, in the December 2017 errata issue.

Polycarbonate Extruded Profile Properties and What the Datasheet Leaves Out

Read the resin sheet for viscosity, heat and growth, then ask what it leaves out about the profile itself.

What a Polycarbonate Datasheet States for Profile GradesTwo documents are read side by side here. SABIC's datasheet for LEXAN 135 resin describes the highest-viscosity linear polycarbonate powder in its range, and it names profile extrusion as the processing method.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote