Meaning
A stress-relieved temper is an aluminum temper for profiles relieved of residual stress, written with 510 or 511 added, as in T6511. The Aluminum Association groups them under the general designations TX510 and TX511. They matter most for parts that will be machined.Two Groups
The TX510 group covers T3510, T4510, T61510, T6510, T8510, T73510 and T76510. The TX511 group covers the same base tempers ending in 511, such as T6511. The two groups are treated differently in the tolerance tables. A drawing names the full temper, and the group name alone is not enough.Read More
Tolerance Effect
For the TX510 tempers, the footnotes leave form tolerances to agreement between purchaser and vendor. Printed rows exist for TX511, among them its own lines in the straightness table. Extruded tube in either group with walls under 2.4 mm (0.095 in) carries no straightness limit.When to Order It
An extrusion carries stress from the quench and the stretch, and machining releases it. For parts that will be machined, or asymmetrical shapes cut to size, the AEC manual recommends one of these tempers when close limits apply. TX511 is the example it gives.On the Drawing
An order for 6082-T6511 is an order for a stress-relieved profile, and a plain T6 delivery falls short of it. The Aluminum Association’s property table lists 6082-T6 and T6511 together, at 262 MPa (38.0 ksi) yield from 5.1 to 19.1 mm. Before writing one, a buyer checks which of these tempers the supplier actually offers in that alloy.Certificate Check
The certificate repeats the temper exactly as ordered. A T6 certificate does not answer an order for T6511. Where the stress relief matters for machining, the drawing and the order both carry the full code.