Meaning

A hollow profile is an extruded section whose walls completely enclose one or more voids along its length. A rectangular tube with an inner web, as in the worked 6082 and 6005A examples, is a typical one. The closed void changes the die, the strength rows, the tolerance tables and, in plastic, the way the section is cooled. A profile that only partly encloses a void is a semihollow, and it is judged by a different rule.

Die and Seam

An aluminum hollow cannot be formed by a flat plate alone. The die is a two-part tool, with a mandrel that shapes the void held on bridges. Metal splits around the bridges, then meets again under pressure in a welding chamber ahead of the bearing. That joint leaves seam lines along the bar. A sound seam is the aim, yet it remains a joint, which matters before a hollow is anodized, bent or pressurized. Hydro notes that these dies take more design and machining, which shows in their lead time.
Read More

Die Life

Hollow dies wear sooner than solid ones at the same wall. The AEC manual gives a hollow die with 1.0 to 1.5 mm walls about 1.1 t (2,500 lb) before its bearing wears, without nitriding. The solid die at that wall lasts about 1.8 t (4,000 lb). Over its whole life, the same hollow die extrudes about 19.1 t against 33.6 t for the solid one. No case in the table wears its bearing sooner than a thin hollow wall.

Property Rows

Hydro’s datasheets for EN AW-6082 and EN AW-6005A print separate rows for open and hollow profiles. For 6082-T6, the hollow thin band runs up to 5 mm (0.20 in) and its upper band ends at 15 mm (0.59 in). The open upper band reaches 25 mm (0.98 in). In 6005A-T6, a hollow with walls up to 5 mm is guaranteed 215 MPa (31.2 ksi) yield. An open profile of the same wall gets 225 MPa (32.6 ksi). The 6063 sheet makes no such split, so its rows serve hollow and open sections alike.

Wall Tolerance

ANSI H35.2-2017 tolerates a wall that completely encloses a space of 71 mm² (0.11 sq in) or more as a percentage. Under a 254 mm (10 in) circumscribing circle it is ±10 %, with a floor of ±0.25 mm (0.010 in). The ceiling is ±1.52 mm (0.060 in). Flatness of a hollow face comes from Table 11.9, whose factors equal or exceed the solid ones in Table 11.8. At a face up to 3.1 mm thick and 203 to 254 mm wide, the factor is 0.012 against 0.010.

Cooling and Calibration

Cooling reaches a plastic hollow only through its outside walls. Heat from inside the section reheats those walls, so the calibrator for a hollow has to be longer. Plastics Technology notes such calibrators once passed 1.8 m (6 ft), which also calls for a long, strong puller. Hollows need wet calibration, often with differential vacuum, so the chambers do not collapse.

Tube or Profile

A hollow part is first sorted into a family of tables. ANSI H35.2 reads extruded profiles from its section 11 tables and extruded tube from section 12. The Aluminum Association points hollow profiles and tube to Tables 11.2, 12.2, 12.3 and 12.4 for cross-section limits. Under ASTM B221 a hollow section is covered as a profile for general purposes. Once it has to carry pressure, the scope sends it to B210 or B241.

Clamping and Machining

A closed chamber deforms under the clamp that holds it for sawing or machining. Saw makers ask for adjustable clamp pressure on thin or hollow profiles. It has to stop movement without crushing the chamber. Clamps close to the cut, on both sides of the blade, keep the falling piece from tilting and tearing an exit burr. Where machined features have to hold close limits, the AEC manual advises a stress-relieved temper, TX511 being its example.

EN 755-9 and EN 12020-2 Scope and Editions for Aluminum Extruded Profiles

Name EN 755-9 or EN 12020-2 with its year, because scope, alloys and limits differ by standard and edition.

What EN 755-9 and EN 12020-2 Each CoverEN 755-9 is part 9 of the EN 755 series for extruded rod and bar, tube and profiles. BSI describes BS EN 755-9:2016 as specifying the tolerances on dimensions and form for aluminum and aluminum alloy profiles with a cross-section contained within a circumscribing circle not greater than 800 mm.

Aluminum Extrusion Die Life in Kilograms Before the Bearing Wears

Die life is counted in tonnes of aluminum before the bearing wears, so a bridge run usually needs one die and a plan for its trial and correction.

What Wears an Extrusion Die and How FastThe AEC manual explains that the life of an extrusion die is generally set by wear of the bearing, the surface of the die opening at right angles to the die face that controls metal flow and velocity by friction. Because the bearing determines the control and finish of the profile, any deterioration, given the finish required, leads to premature failure of the die.

How Much of an Aluminum Billet Becomes Shipped Profile

Order weight, butt, stretcher ends and rejects decide how many billets a small aluminum extrusion run takes and what the buyer receives.

The Yield Stack From Billet to Shipped LengthA billet is heated, pushed through a die, quenched, stretched, sawn and aged. Metal leaves the stream at three points, and each has a figure in the published sources.

Plastic Profile Extrusion Line From Die Lip to Cut Length

A profile die only suggests the shape, and the sizer, puller and saw that follow have to hold the size until the plastic is solid.

The Stations of a Plastic Profile Line From Hopper to SawA typical line has five parts: an extruder, a die with its adapter, sizing and cooling equipment, a puller, and a way to cut the profile to length. The same five appear in a rigid vinyl guide from a PVC compound maker.

Cutting and Machining Extruded Aluminum Lengths

A press saw makes bars into shippable lengths, and a precision saw with the right blade, clamps and datums makes the length the drawing asks for.

The Order of Operations From Bar to Cut LengthCutting comes first in almost any fabrication plan, with deburring and then drilling, punching or machining after it. A burr left from the cut sits where the clamp has to hold the piece for the next step, so the order carries weight.

Aluminum Extrusion Process From Billet to Aged Profile

The press pushes a softened billet through a die, and the quench, stretch and oven that follow decide whether the bar is straight and strong.

The Steps of Aluminum Extrusion in the Order the Metal Meets ThemSeven operations turn a cast billet into a profile ready for finishing. A billet is a solid cylinder of cast aluminum, and it never melts on the way.

Straightness, Twist and Flatness Tolerance of Aluminum Extrusions

Form limits scale with length and width, so work them out for the real length before accepting a drawing.

The Straightness Limit and Its FormulaTable 11.6 of Aluminum Standards and Data, in the May 2009 reprint, gives the allowable deviation D from straight in inches. For profiles the limit is a factor multiplied by the measured length in feet, and it applies in total length or in any measured segment of one foot or more of the total length.

ANSI H35.2 Standard Tolerances for Aluminum Extrusions

Name the edition and the class on the drawing, because the standard column governs when nothing is written.

What ANSI H35.2 Covers and How to Cite ItThe title is American National Standard Dimensional Tolerances for Aluminum Mill Products, and the Aluminum Association is its secretariat. Opened for this piece was ANSI H35.2-2017, approved May 12, 2017 as a revision of the 2013 edition, in the December 2017 errata issue.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote