EN 755-2

EN 755-2 is the European standard that sets the minimum mechanical properties of extruded aluminum products, profiles included.

Every EN 755-2 article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

EN 755-2 is the European standard that sets the minimum mechanical properties of extruded aluminum products, profiles included. Hydro’s alloy datasheets quote it in its 2016 edition. Its limits are in MPa and its thickness bands in millimeters. A European certificate for an extruded profile is read against it.

What It Lists

Each row ties a minimum yield, tensile strength and elongation to an alloy, a temper and a wall band. For EN AW-6063 in T6, walls up to 10 mm (0.39 in) are guaranteed 170 MPa (24.7 ksi) yield. Open EN AW-6082-T6 sections up to 5 mm (0.20 in) get 250 MPa (36.3 ksi). For some alloys, open and hollow sections get separate rows. A footnote makes the lowest band value govern a section that spans two bands.
Read More

Companion Standards

EN 755-2 sits in a family of European documents. Composition limits come from EN 573-3, and temper definitions from EN 515. Dimensional and form tolerances for profiles sit in EN 755-9. One enclosure maker cites EN 12020-2 for its precision aluminum profiles.

On the Order

A typical order line pairs the two, as in EN AW-6005A to EN 755-2. It adds the temper, whether the section is open or hollow, and the thickest wall. With those, the certificate and the drawing point to the same row. Hydro’s special variants, such as its 6082 T66, sit outside the standard rows and are agreed with the producer.

Against the Inch Tables

The Aluminum Association’s North American limits are a separate set with different band edges. Its 6063-T6 yield limit is 172 MPa (25.0 ksi), close to the European 170 MPa but on other thickness bands. A lot that meets one table may miss the other. One governing standard is named on the order.

ASTM B221 for Extruded Aluminum Profiles Read for the Buyer

The specification certifies alloy, temper and tensile behavior, so the drawing still has to carry geometry, units and thickness.

What ASTM B221 CoversASTM's catalog page for B221-21, last updated October 29, 2021, describes the standard as a specification for aluminum and aluminum-alloy extruded bars, rods, wire, profiles and tubes. It covers the alloys and tempers listed in its Table 2 and requires the products to be made by hot extrusion or a similar process.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote