6082

Alloy 6082 is the strongest grade in Hydro's grading of common 6000-series extrusion alloys, designated EN AW-6082 or AlSi1MgMn. Its manganese is there for toughness.

Every 6082 article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Alloy 6082 is the strongest grade in Hydro’s grading of common 6000-series extrusion alloys, designated EN AW-6082 or AlSi1MgMn. Its manganese is there for toughness. Beams, bumper rails, scaffolding and train floors appear among the maker’s listed uses. It trades surface finish and anodizing quality for strength and machinability.

Composition

Hydro gives silicon at 0.70 to 1.30 % and magnesium at 0.60 to 1.20 %. Manganese runs from 0.40 to 1.00 %, iron reaches 0.50 % and chromium 0.25 %. That is roughly twice the silicon of 6063. According to Hydro, that manganese is what costs the alloy its decorative anodizing quality.
Read More

Strength Rows

An open 6082-T6 profile up to 5 mm (0.20 in) is guaranteed 250 MPa (36.3 ksi) yield and 290 MPa (42.1 ksi) tensile. From 5 to 25 mm the figures rise to 260 and 310 MPa (37.7 and 45.0 ksi). Hollow profiles follow the same values, with the upper band ending at 15 mm. T4 is guaranteed 110 MPa (16.0 ksi) yield. Hydro also offers a special T66 at 320 MPa (46.4 ksi), outside the standard rows.

Inch Table

The Aluminum Association’s table lists 6082-T6 and the stress-relieved T6511 together. From 5.1 to 19.1 mm (0.200 to 0.750 in) they carry 262 MPa (38.0 ksi) yield and 310 MPa (45.0 ksi) tensile. Its rows run to 203 mm (8 in) of thickness, far past the 25 mm of the European sheet. In its thickest band, 152 to 203 mm, yield falls to 241 MPa (35.0 ksi).

Grades and Uses

Hydro’s relative scale grades 6082 at 4 for tensile strength and 5 for machinability. Weldability is 4, cold forming 3, and surface finish and decorative anodizing 2 each. A painted or hidden structural part loses little from the low finish grades. A machined block or a load-carrying rail suits it, and a visible anodized face does not.

Next to 6063

Against 6063-T6, the guaranteed yield of 6082-T6 is about 47 % higher. Thermal conductivity falls from 201 to 172 W/m·K, about 14 %. Stiffness barely moves, at 70 GPa (10.2 Msi) against 69 GPa. Density is 2.71 g/cm³ (0.098 lb/in³), and the melting range runs from 575 to 650 °C (1,067 to 1,202 °F).

ASTM B221 for Extruded Aluminum Profiles Read for the Buyer

The specification certifies alloy, temper and tensile behavior, so the drawing still has to carry geometry, units and thickness.

What ASTM B221 CoversASTM's catalog page for B221-21, last updated October 29, 2021, describes the standard as a specification for aluminum and aluminum-alloy extruded bars, rods, wire, profiles and tubes. It covers the alloys and tempers listed in its Table 2 and requires the products to be made by hot extrusion or a similar process.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote