Surface Finish

Surface finish is the quality of an extruded profile's surface as it leaves the die, graded by alloy and governed by the die bearing.

Every Surface Finish article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Surface finish is the quality of an extruded profile’s surface as it leaves the die, graded by alloy and governed by the die bearing. It matters most where a face is seen or anodized. It also costs die life, since a demanding finish wears a die out sooner.

Alloy Grades

Hydro’s relative scale, with 5 at the top, grades surface finish 5 for 6060 and 4 for 6063. Alloys 6005 and 6005A grade 3, and 6082 grades 2. Hydro’s text describes 6060 as replacing 6063 for its improved finish. It calls 6005A a good mix of strength, toughness and surface finish.
Read More

Role of the Die

The AEC manual places finish control in the die bearing. Because the bearing sets both the control and the finish of the profile, its wear ends a die’s useful life early when finish matters. Hydro adds that a high surface finish is one of the features that lengthen die design. Its die correction aims at agreed surface targets as well as tolerances.

Effect on Die Life

The die life figures in the AEC table assume mill finish. A visible or decorative finish therefore uses up a bearing faster than the table shows. A buyer treats the table as an upper bound when the finish is demanding. The die plan for a run states the finish it was made for.

Choosing the Alloy

Hydro’s own grades point to 6060 when the seen face decides. Where guaranteed strength decides it, the table favors 6063. A structural face that is painted or hidden loses little with 6082. The choice is written on the order with the finish named.

Aluminum Extrusion Die Life in Kilograms Before the Bearing Wears

Die life is counted in tonnes of aluminum before the bearing wears, so a bridge run usually needs one die and a plan for its trial and correction.

What Wears an Extrusion Die and How FastThe AEC manual explains that the life of an extrusion die is generally set by wear of the bearing, the surface of the die opening at right angles to the die face that controls metal flow and velocity by friction. Because the bearing determines the control and finish of the profile, any deterioration, given the finish required, leads to premature failure of the die.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote