Impact

Impact resistance is a material's or coating's ability to absorb a sudden blow without cracking or losing adhesion, measured by notched bar, falling weight or drop dart tests.

Every Impact article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Impact resistance is a material’s or coating’s ability to absorb a sudden blow without cracking or losing adhesion, measured by notched bar, falling weight or drop dart tests.

Aluminum Alloys

Hydro’s relative grading, with 5 the top grade, rates impact strength at 2 for 6060 and 6063, 1 for 6005, 3 for 6005A and 4 for 6082.
Read More

Rigid PVC

Rigid PVC compounds carry impact modifiers for toughness, and ASTM D1784 classifies them by notched impact among its properties. NETZSCH links the degree of gelation directly to impact strength. A drawdown that is too large leaves high residual stress and brittleness on impact, which is why rigid PVC tolerates only 4 to 10 % drawdown in the cited guidance.

Polycarbonate

Covestro prints notched Izod impact strength of 70 kJ/m2 at 23 °C and 20 kJ/m2 at -30 °C on 3 mm specimens for one extrusion grade, with Charpy notched impact of 80 and 18 kJ/m2.

Coatings

The PCI comparison lists a Qualicoat impact of 2.5 N·m (22 in·lb) to ASTM D2794 with no cracking or detachment, and an AAMA direct impact to ASTM D5420 with 3 mm deformation and no removal of coating.

Specification

Impact values depend on the specimen, the notch and the temperature, so they are compared only under the same method.

Low Temperature

Impact values fall in the cold. The polycarbonate grade’s notched Izod drops from 70 to 20 kJ/m2 between 23 and -30 °C (73 and -22 °F), while its puncture energy rises from 60 to 70 J. A part that sees winter service is judged at its lowest temperature.

Qualicoat and AAMA 2603 to 2605 Coating Specifications for Aluminum Extrusions

Name the Qualicoat class or AAMA tier on the drawing, then fix the approved sample, channel thickness and machining rules that neither standard settles.

What Qualicoat and AAMA 2603, 2604 and 2605 CoverQualicoat is a quality label for coatings on aluminum for architectural use. Its 26th edition, introduced in the document QCT-INTRO-26 valid from 1 January 2026, splits the specifications into three volumes: one for coaters, one for makers of chemical pretreatments and one for powder makers.

Rigid PVC Compounds for Extruded Profiles

Rigid PVC profiles are stiff and easy to extrude, but their glass transition sets the heat limit, so name service temperature and color with the compound.

What a Rigid PVC Extrusion Compound ContainsRigid PVC, also written PVC-U for unplasticized, is polyvinyl chloride without plasticizer. It is never extruded as bare resin.

Plastic Profile Extrusion Line From Die Lip to Cut Length

A profile die only suggests the shape, and the sizer, puller and saw that follow have to hold the size until the plastic is solid.

The Stations of a Plastic Profile Line From Hopper to SawA typical line has five parts: an extruder, a die with its adapter, sizing and cooling equipment, a puller, and a way to cut the profile to length. The same five appear in a rigid vinyl guide from a PVC compound maker.

Polycarbonate Extruded Profile Properties and What the Datasheet Leaves Out

Read the resin sheet for viscosity, heat and growth, then ask what it leaves out about the profile itself.

What a Polycarbonate Datasheet States for Profile GradesTwo documents are read side by side here. SABIC's datasheet for LEXAN 135 resin describes the highest-viscosity linear polycarbonate powder in its range, and it names profile extrusion as the processing method.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.