Thin Wall

A thin wall is a profile wall slender enough to change the rules that apply to it, as at 2.4 mm (0.094 in).

Every Thin Wall article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A thin wall is a profile wall slender enough to change the rules that apply to it, as at 2.4 mm (0.094 in). Thin walls raise the straightness allowance, the relative tolerance and the die risk. They also need gentler handling at the saw and in the machine.

Straightness Allowance

The Aluminum Association counts a small profile as thin-walled when a third or more of its perimeter is 2.4 mm metal or less. Such a profile gets 4.17 mm per meter (0.050 in per foot) of straightness. A stout profile gets 1.04 mm per meter (0.0125 in per foot). Over 6 m (19.7 ft) the thin profile may bow 25 mm (0.98 in).
Read More

Relative Tolerance

Thin walls carry the largest tolerance as a share of their size. In ANSI H35.2-2017 a wall enclosing a void has a floor of ±0.25 mm (0.010 in). On a 1.5 mm (0.06 in) wall that floor is a sixth of the thickness. BWF’s plastic table gives walls up to 1.2 mm (0.047 in) ±0.2 mm, about 17 %. Closer relative limits on such walls are negotiated while the die design is still open.

Die Risk

Thin walls shorten die life and raise the risk of die damage. In the AEC table a hollow die with 1.0 to 1.5 mm walls has the shortest first bearing life of any row. The AEC manual adds that thin walls with demanding tongue ratios may need custom tooling. Without it, the die can deflect, break or miss its tolerances.

Plastic Land

A plastic die land is normally 10 times the wall. Plastics Technology warns that the ratio can build too much pressure when a stiff melt has to fill a slender wall. Its stated ceiling for continuous backpressure is about 34.5 MPa (5,000 psi). Typical profile walls in the same source run from 1 to 3 mm.

Cutting Thin Walls

A blade with many teeth keeps several of them on a thin wall at once. The wall then has no room to bend between teeth. Clamp pressure on thin or hollow sections is adjustable. In machining, thin sections are where chatter and rough walls appear in slots and pockets.

Anodizing Extruded Aluminum Profiles Step by Step

Anodizing an extrusion is a line of tanks, and the rack, etch, bath, color and seal each leave their own mark on the profile.

The Anodizing Line From Rack to SealHydro's anodizing brochure for extruded profiles lays out the line in the order the profiles travel. The Aluminum Anodizers Council groups the same work into five stages: cleaning, pretreatment, anodizing, coloring and sealing.

Aluminum Extrusion Die Life in Kilograms Before the Bearing Wears

Die life is counted in tonnes of aluminum before the bearing wears, so a bridge run usually needs one die and a plan for its trial and correction.

What Wears an Extrusion Die and How FastThe AEC manual explains that the life of an extrusion die is generally set by wear of the bearing, the surface of the die opening at right angles to the die face that controls metal flow and velocity by friction. Because the bearing determines the control and finish of the profile, any deterioration, given the finish required, leads to premature failure of the die.

Plastic Profile Extrusion Line From Die Lip to Cut Length

A profile die only suggests the shape, and the sizer, puller and saw that follow have to hold the size until the plastic is solid.

The Stations of a Plastic Profile Line From Hopper to SawA typical line has five parts: an extruder, a die with its adapter, sizing and cooling equipment, a puller, and a way to cut the profile to length. The same five appear in a rigid vinyl guide from a PVC compound maker.

Cutting and Machining Extruded Aluminum Lengths

A press saw makes bars into shippable lengths, and a precision saw with the right blade, clamps and datums makes the length the drawing asks for.

The Order of Operations From Bar to Cut LengthCutting comes first in almost any fabrication plan, with deburring and then drilling, punching or machining after it. A burr left from the cut sits where the clamp has to hold the piece for the next step, so the order carries weight.

Wall Thickness and Cross-Section Tolerance of Extruded Plastic Profiles

Read the nominal size row for each dimension, then check the fit as a sum of limits, not a single one.

Cross-Section Dimension Limits by Nominal SizeBWF's quality, tolerance and processing guidelines of 20 November 2024 apply limit values according to DIN 16941, series 2A and 2B, unless the drawing says otherwise. The general tolerances apply at any point of the profile cross-section, seen at right angles to the extrusion direction.

ANSI H35.2 Standard Tolerances for Aluminum Extrusions

Name the edition and the class on the drawing, because the standard column governs when nothing is written.

What ANSI H35.2 Covers and How to Cite ItThe title is American National Standard Dimensional Tolerances for Aluminum Mill Products, and the Aluminum Association is its secretariat. Opened for this piece was ANSI H35.2-2017, approved May 12, 2017 as a revision of the 2013 edition, in the December 2017 errata issue.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.