Yield Strength

Yield strength is the stress at which an aluminum profile starts to deform permanently, written Rp0.2 on European datasheets.

Every Yield Strength article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Yield strength is the stress at which an aluminum profile starts to deform permanently, written Rp0.2 on European datasheets. It is the guaranteed figure most structural designs and certificates lean on. Tables give it as a minimum for each alloy, temper and thickness band.

Guaranteed Values

Hydro’s EN 755-2 figures for 6063 up to 10 mm (0.39 in) climb with temper. T4 gives 65 MPa (9.4 ksi), T5 130 MPa (18.9 ksi) and T6 170 MPa (24.7 ksi). An open 6082-T6 section reaches 250 MPa (36.3 ksi) up to 5 mm and 260 MPa (37.7 ksi) above. A 6005A-T6 section falls from 225 MPa (32.6 ksi) to 200 MPa (29.0 ksi) as its walls thicken.
Read More

Alloy Ladder

The Aluminum Association’s table gives a ladder of minimum yields for thin to moderate walls. The ladder starts with 6063-T6 at 172 MPa (25.0 ksi), then 6061-T6 at 241 MPa (35.0 ksi). Next comes 6082-T6 at 262 MPa (38.0 ksi). At the top, 7075-T6 is listed at 483 MPa (70.0 ksi). Elongation floors fall as the ladder climbs.

Stiffness Is Separate

A higher yield does not make a profile stiffer. Hydro gives 6063 a modulus of 69 GPa (10.0 Msi), and both structural alloys 70 GPa (10.2 Msi). Moving from 6063-T6 to 6082-T6 raises yield by about 47 %, yet deflection under the same load barely changes. Where deflection is the limit, the stronger alloy brings no benefit.

At the Stretcher

Yield strength also sets the force the process needs. A University of Illinois thesis sets the minimum stretcher force at section area multiplied by yield strength. Grip pressure is held in a window where the jaws neither slide nor flatten the profile.

At a Weld

The guaranteed yield belongs to the profile as tempered. Welding heat changes the temper near the joint, so the table figure does not apply there. The datasheets print no welded-joint strengths, and those values come from the supplier or the fabricator.

Aluminum Extrusion Process From Billet to Aged Profile

The press pushes a softened billet through a die, and the quench, stretch and oven that follow decide whether the bar is straight and strong.

The Steps of Aluminum Extrusion in the Order the Metal Meets ThemSeven operations turn a cast billet into a profile ready for finishing. A billet is a solid cylinder of cast aluminum, and it never melts on the way.

ASTM B221 for Extruded Aluminum Profiles Read for the Buyer

The specification certifies alloy, temper and tensile behavior, so the drawing still has to carry geometry, units and thickness.

What ASTM B221 CoversASTM's catalog page for B221-21, last updated October 29, 2021, describes the standard as a specification for aluminum and aluminum-alloy extruded bars, rods, wire, profiles and tubes. It covers the alloys and tempers listed in its Table 2 and requires the products to be made by hot extrusion or a similar process.

6063 Aluminum Extrusion Properties in T5 and T6

Read the temper, the thickest wall and the word minimum before trusting any strength figure for this alloy.

What EN AW-6063 Guarantees in T4, T5, T6 and T66Hydro's datasheet for EN AW-6063 (alloy designation AlMg0.7Si) lists minimum mechanical properties taken from EN 755-2:2016 for extruded profile. The values are minimums, and each row is tied to a wall thickness band.

Send the Section Drawing of Your Profile