Moisture is the water a plastic profile or its resin takes up from the air or from storage.

Every Moisture article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Moisture is the water a plastic profile or its resin takes up from the air or from storage. In the resin it disturbs the melt, and in the finished profile it changes length. Aluminum is not affected in this way, so moisture is a plastic subject. Polycarbonate, PMMA and the polyamides are the materials the sources name.

Uptake

Polycarbonate takes up little water, but the amount is measurable. SABIC’s LEXAN 135 sheet gives 0.15 % at equilibrium in air at 23 °C (73 °F) and 50 % relative humidity. Fully immersed, it reaches 0.35 % at saturation. Covestro gives 0.12 % and 0.3 % for Makrolon ET3113. Both figures are small, yet SABIC still asks for hours of drying before processing.
Read More

In the Melt

Moisture thins the melt. Newey’s process paper links that to surface imperfections and size variation along the run. Hygroscopic materials are therefore dried continuously through a dehumidifying dryer. Polyamides absorb water so quickly that they are fed on a closed loop.

Drying

Drying times sit on the resin sheet. SABIC lists 2 to 4 hours at 120 °C (248 °F) for LEXAN 135 before processing. A Teknor Apex guide says rigid PVC pellets typically need no drying. Where drying is still wanted, its figure is 49 °C (120 °F) for 2 to 3 hours. A quote for a polycarbonate profile that omits drying has left out a step.

Effect on Length

BWF notes that profiles absorb moisture according to storage and ambient conditions, and that length follows. Faces kept in different conditions can change unevenly and show waves or bulges. BWF’s lengths are defined at 20 °C (68 °F) and 30 % relative humidity. Its storage advice is to keep profiles lying flat, near 20 °C and 50 % humidity. A length measured after damp storage is compared with the drawing only after the profile is back at those conditions.

Before the Run

Moisture is one of the supply questions settled before a plastic line starts. Dryers sit beside the extruder, the die, the sizer, the puller and the saw as services every line needs. SABIC also lists a hopper temperature of 40 to 60 °C (104 to 140 °F) for LEXAN 135. Dried powder stays warm on its way to the screw. A run’s opening hour goes on getting such conditions right: dry material, steady water, a hot die and a puller at speed.

In the Quote

Drying is the line most often missing from a quotation for a polycarbonate profile. Its 2 to 4 hours at 120 °C (248 °F) are real line time and energy. A quote that names the resin grade also names the drying step that grade requires.

In Storage

Moisture keeps acting after the profile leaves the line. A profile stored at a humidity other than the agreed reference drifts in length. No saw table allows for that drift. Faces that see different conditions, such as one side against a wall, can change unevenly. Flat storage at stable temperature and humidity keeps the length predictable.

In Inspection

A receiving check on plastic lengths follows the reference conditions. The inspection plan states the temperature of measurement, and the profile is conditioned before it is measured. Where a lot has been stored damp, the conditioning time goes into the plan. Without that step, a correct profile can be rejected and a wrong one accepted.

Hygroscopic Grades

The sources treat some materials as far more sensitive than others. Newey singles out the polyamides, which absorb water so quickly that they are fed on a closed loop from the dryer. Polycarbonate needs drying but takes up little water at equilibrium. Rigid PVC pellets usually need none. The resin sheet for each grade says which case applies.

Rigid PVC Compounds for Extruded Profiles

Rigid PVC profiles are stiff and easy to extrude, but their glass transition sets the heat limit, so name service temperature and color with the compound.

What a Rigid PVC Extrusion Compound ContainsRigid PVC, also written PVC-U for unplasticized, is polyvinyl chloride without plasticizer. It is never extruded as bare resin.

Planning a Plastic Profile Extrusion Run From Die Trial to Regrind

A plastic profile run is a tooling set tied to one resin, a trial that makes scrap, and steady hours that arithmetic on kilograms per hour can size.

What a Plastic Profile Run Is Made OfFour parts make a run: the tooling set, the start-up, the steady production and the changeover at the end. Each has its own tool, its own time and its own scrap, and a buyer who plans a quantity needs to ask about all four.

Plastic Profile Extrusion Line From Die Lip to Cut Length

A profile die only suggests the shape, and the sizer, puller and saw that follow have to hold the size until the plastic is solid.

The Stations of a Plastic Profile Line From Hopper to SawA typical line has five parts: an extruder, a die with its adapter, sizing and cooling equipment, a puller, and a way to cut the profile to length. The same five appear in a rigid vinyl guide from a PVC compound maker.

Wall Thickness and Cross-Section Tolerance of Extruded Plastic Profiles

Read the nominal size row for each dimension, then check the fit as a sum of limits, not a single one.

Cross-Section Dimension Limits by Nominal SizeBWF's quality, tolerance and processing guidelines of 20 November 2024 apply limit values according to DIN 16941, series 2A and 2B, unless the drawing says otherwise. The general tolerances apply at any point of the profile cross-section, seen at right angles to the extrusion direction.

Cut Length and Saw Cut Tolerance of Extruded Profiles

A length tolerance belongs to a cutting step and a measuring method, so name both with the number.

Saw Tolerances for Plastic Profile LengthsBWF's guidelines of 20 November 2024 give saw tolerances for polycarbonate and PMMA profiles in two cases, offline cut and inline cut. Each is tabulated against the length, in millimeters, and each is tied to a method: lengths up to 4,500 mm are measured on a measuring table that checks length and angle, and longer ones with a measuring tape.

DIN 16941 General Tolerances for Extruded Plastic Profiles

Cite the edition and the series on the drawing, then add what the general tolerances leave open.

What DIN 16941 CoversThe current edition is DIN 16941:2012-11, titled Thermoplastics extruded profiles, General tolerances of size, form and orientation, with the German title Extrudierte Profile aus thermoplastischen Kunststoffen, Allgemeintoleranzen für Maße, Form und Lage. It is published in German, with an English translation sold separately, and it replaces DIN 16941:1986-05.

Polycarbonate Extruded Profile Properties and What the Datasheet Leaves Out

Read the resin sheet for viscosity, heat and growth, then ask what it leaves out about the profile itself.

What a Polycarbonate Datasheet States for Profile GradesTwo documents are read side by side here. SABIC's datasheet for LEXAN 135 resin describes the highest-viscosity linear polycarbonate powder in its range, and it names profile extrusion as the processing method.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote