Die Lines

Die lines are fine marks running along the length of an extruded profile, left by the die opening as material passes through it.

Every Die Lines article of the Profile Extrusion Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Die lines are fine marks running along the length of an extruded profile, left by the die opening as material passes through it. They appear on aluminum and plastic profiles alike. Standards limit their depth on aluminum, and process guides trace their causes on plastic.

Aluminum Depth Limit

Table 11.10 of the Aluminum Association caps how deep die lines and handling marks may be. For section thickness up to 1.6 mm (0.063 in) the allowed depth is 0.04 mm (0.0015 in). Between 6.4 and 12.7 mm (0.25 and 0.50 in) it is 0.10 mm (0.004 in). Above 12.7 mm it is 0.20 mm (0.008 in). The deeper allowance on thick sections reflects the scale of the part.
Read More

Plastic Causes

A rigid vinyl processing guide lists die lines among its troubleshooting symptoms. It traces them to a nicked die approach or to plate-out on the tooling. A process planner reads die lines as a sign that the die needs attention. They are one of the faults a die trial is meant to find before the production run.

Correction

The same guide gives three remedies. The die is polished, brass tools are used near it so its surfaces are not nicked, and the line runs colder. A die cut for one compound and run hot for output may show lines that a cooler setting removes.

Visible Faces

On a clear profile, lines matter to the eye. BWF does not allow extrusion lines on the visible surface unless the extrusion process itself causes them. Its inspection looks at the face from about 1 m (3.3 ft), with and without light. The drawing or the surface agreement says which faces are visible.

Anodizing Extruded Aluminum Profiles Step by Step

Anodizing an extrusion is a line of tanks, and the rack, etch, bath, color and seal each leave their own mark on the profile.

The Anodizing Line From Rack to SealHydro's anodizing brochure for extruded profiles lays out the line in the order the profiles travel. The Aluminum Anodizers Council groups the same work into five stages: cleaning, pretreatment, anodizing, coloring and sealing.

Anodized Film Thickness and Color Tolerance on Extruded Profiles

Specify anodic film as an ISO 7599 class on marked faces, and agree color against limit samples before the first lot is anodized.

How Anodized Film Thickness Is Specified and AcceptedISO 7599:2018, published in Europe as EN ISO 7599:2018 and in Britain as BS EN ISO 7599:2018, lays down the method. Its contents run from the information the customer supplies to the anodizer, through coating thickness, sealing, appearance and color, to a normative annex on interpreting average and local thickness.

Planning a Plastic Profile Extrusion Run From Die Trial to Regrind

A plastic profile run is a tooling set tied to one resin, a trial that makes scrap, and steady hours that arithmetic on kilograms per hour can size.

What a Plastic Profile Run Is Made OfFour parts make a run: the tooling set, the start-up, the steady production and the changeover at the end. Each has its own tool, its own time and its own scrap, and a buyer who plans a quantity needs to ask about all four.

Plastic Profile Extrusion Line From Die Lip to Cut Length

A profile die only suggests the shape, and the sizer, puller and saw that follow have to hold the size until the plastic is solid.

The Stations of a Plastic Profile Line From Hopper to SawA typical line has five parts: an extruder, a die with its adapter, sizing and cooling equipment, a puller, and a way to cut the profile to length. The same five appear in a rigid vinyl guide from a PVC compound maker.

Straightness, Twist and Flatness Tolerance of Aluminum Extrusions

Form limits scale with length and width, so work them out for the real length before accepting a drawing.

The Straightness Limit and Its FormulaTable 11.6 of Aluminum Standards and Data, in the May 2009 reprint, gives the allowable deviation D from straight in inches. For profiles the limit is a factor multiplied by the measured length in feet, and it applies in total length or in any measured segment of one foot or more of the total length.

ANSI H35.2 Standard Tolerances for Aluminum Extrusions

Name the edition and the class on the drawing, because the standard column governs when nothing is written.

What ANSI H35.2 Covers and How to Cite ItThe title is American National Standard Dimensional Tolerances for Aluminum Mill Products, and the Aluminum Association is its secretariat. Opened for this piece was ANSI H35.2-2017, approved May 12, 2017 as a revision of the 2013 edition, in the December 2017 errata issue.

Send the Section Drawing of Your Profile

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Profile Extrusion chosen.

Request a Quote